Abstract :K418 Ni-base superalloy was melted in high vacuum arc-melting furnace.

采用高真空电弧熔炼炉熔炼,制备了K418镍基高温合金。

The effects of strain rate on the matrix and precipitate phases of Ni-base superalloy have been analyzed using the theory.

结果表明,镍基单晶基体相和强化相均表现出明显的率相关性。

The effect of melt overheating treatment on the solidification segregation of M963 cast Ni-base superalloy has been studied.

研究了熔体过热处理对M963铸造镍基高温合金凝固偏析的影响。

An investigation of the surface of Ni-base superalloy powder particles in both as-atomized and as-HIP' ed conditions has been presented in the paper.

本文介绍了用扫描电子显微镜和俄歇电子谱仪观察和分析雾化态和热等静压态高温合金粉末颗粒的表面。

The elimination of defects and the improvement in microstructure and mechanical properties of a east Ni-base superalloy treated with hot isostatic pressing (HIP) have been investigated.

就热等静压处理对镍基铸造高温合金的缺陷消除、组织和力学性能的改善作了研究。

The liquid structure and melt treatment of M963 Ni base superalloy have been studied by using high temperature X-ray diffraction.

通过液态X射线衍射研究了铸态镍基高温合金M 963的液态结构和熔体处理。